{"id":367,"date":"2016-06-02T19:52:03","date_gmt":"2016-06-02T19:52:03","guid":{"rendered":"http:\/\/www.wyomingtestfixtures.com\/?page_id=367"},"modified":"2024-08-19T16:12:52","modified_gmt":"2024-08-19T22:12:52","slug":"celanese-compression-test-fixture-formerly-astm-d-3410","status":"publish","type":"page","link":"https:\/\/wyomingtestfixtures.com\/de\/products\/compression\/celanese-compression-test-fixture-formerly-astm-d-3410\/","title":{"rendered":"Celanese Druckpr\u00fcfvorrichtung (ehemals ASTM D3410)"},"content":{"rendered":"<h2>Celanese Druckpr\u00fcfvorrichtung (ehemals ASTM D3410)<\/h2>\n<h4>Modell Nr. WTF-CE (Edelstahl)<\/h4>\n\t\t\t\t<img fetchpriority=\"high\" decoding=\"async\" src=\"https:\/\/wyomingtestfixtures.com\/wp-content\/uploads\/2020\/01\/IMG_3363-1024x683.jpg\" alt=\"IMG_3363\" itemprop=\"image\" height=\"467\" width=\"700\" title=\"IMG_3363\" onerror=\"this.style.display='none'\"  \/>\n\t<p>Abb. 1: Explosionszeichnung der Celanese Druckpr\u00fcfvorrichtung.<\/p>\n\t<p>Das Celanese Compression Test Fixture wurde erstmals von I.K. Park von der Celanese Corporation im Jahr 1971 vorgestellt (Referenz 1).  Sie wurde 1975 als ASTM-Norm D3410 angenommen (Verweis 2).  Seitdem wurden jedoch mehrere verbesserte Druckvorrichtungen entwickelt. Daher wurde die Celanese-Vorrichtung im Jahr 2003 aus der ASTM-Norm D3410 gestrichen.<\/p>\n\t<p>Die beiden H\u00e4lften jedes Keilklemmhalters werden zusammengeschraubt, nachdem die Probe dazwischen eingelegt wurde, wobei die mitgelieferte Distanzstange zur Festlegung der Messl\u00e4nge verwendet wird. Die Gesamtausrichtung der Vorrichtungsh\u00e4lften wird durch eine eng anliegende H\u00fclse unterst\u00fctzt, die nach der Installation der Probe \u00fcber die Baugruppe gleitet, aber auch eine potenzielle Quelle f\u00fcr Bindung ist.<\/p>\n\t<p>Die Celanese-Vorrichtung ist sehr kompakt und wiegt etwa 10 lb. Sie wird jedoch h\u00e4ufig wegen der Kegel-in-Kegel-Anordnung der Keilspannzeuge kritisiert.  Um einen vollst\u00e4ndigen Oberfl\u00e4chenkontakt zwischen jedem Paar geteilter Halbkegel und den dazugeh\u00f6rigen konischen Vertiefungen in den Endbl\u00f6cken zu gew\u00e4hrleisten, m\u00fcssen die Laschenenden der Probe mit einer genauen Dicke hergestellt werden, d. h. eine Gesamtdicke an den Laschenenden der Probe von 0,157 Zoll \u00b1 0,002 Zoll. Diese erforderliche Pr\u00e4zision erfordert im Wesentlichen das Schleifen der Oberfl\u00e4che der Laschen nach dem Verkleben mit der Probe. Dies erh\u00f6ht die Zeit und die Kosten der Probenvorbereitung.<\/p>\n\t<p>Bei der Standardvorrichtung werden die Feilenfl\u00e4chen als Greiffl\u00e4chen verwendet. Das hei\u00dft, ein Abschnitt einer echten Metallbearbeitungsfeile wird in einen Schlitz in jedem Keilgriff gedr\u00fcckt. Alternativ k\u00f6nnen auch maschinell bearbeitete Zacken oder mit Wolframkarbidpartikeln beschichtete Oberfl\u00e4chen verwendet werden. Die beiden letztgenannten Arten von Oberfl\u00e4chen werden \u00fcblicherweise bei anderen Zug- und Druckgriffen verwendet.<\/p>\n\t<p><strong>Quellen f\u00fcr zus\u00e4tzliche Informationen:<\/strong><\/p>\n<p>1) I.K. Park, \"Tensile and Compressive Test Methods for High-Modulus Graphite Fibre-Reinforced Composites\", Proceedings of the International Conference on Carbon Fibres, Their Composites and Applications, Paper No. 23, The Plastics Institute, London, 1971.<\/p>\n<p>2) ASTM-Norm D3410-03 (neu genehmigt 2008), \"Compressive Properties of Polymer Matrix Composite Materials with Unsupported Gage Section by Shear Loading\" (Druckeigenschaften von Polymermatrix-Verbundwerkstoffen mit freitragendem DMS-Abschnitt durch Scherbelastung), American Society for Testing and Materials, West Conshohocken, Pennsylvania (erstmals 1975 ver\u00f6ffentlicht).<\/p>\n<p>3) D.F. Adams, \"Current Status of Compression Testing of Composite Materials\", Proceedings of the 40th International SAMPE Symposium, Anaheim, California, Mai 1995, S. 1831-1843.<\/p>","protected":false},"excerpt":{"rendered":"<p>Celanese Compression Test Fixture (ehemals ASTM D3410) Modell Nr. WTF-CE (Edelstahl) Abb. 1: Explosionszeichnung des Celanese Compression Test Fixture. Das Celanese Compression Test Fixture wurde erstmals 1971 von I.K. Park von der Celanese Corporation vorgestellt (Referenz 1).  Sie wurde 1975 als ASTM-Norm D3410 angenommen (Verweis 2).  Es wurden jedoch mehrere verbesserte...<\/p>","protected":false},"author":1,"featured_media":0,"parent":187,"menu_order":6,"comment_status":"closed","ping_status":"closed","template":"full-width-page.php","meta":{"_monsterinsights_skip_tracking":false,"_monsterinsights_sitenote_active":false,"_monsterinsights_sitenote_note":"","_monsterinsights_sitenote_category":0,"footnotes":""},"class_list":["post-367","page","type-page","status-publish","hentry"],"_links":{"self":[{"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/pages\/367","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/comments?post=367"}],"version-history":[{"count":11,"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/pages\/367\/revisions"}],"predecessor-version":[{"id":3767,"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/pages\/367\/revisions\/3767"}],"up":[{"embeddable":true,"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/pages\/187"}],"wp:attachment":[{"href":"https:\/\/wyomingtestfixtures.com\/de\/wp-json\/wp\/v2\/media?parent=367"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}